FIELD: manufacture of alphanumeric and graphical information display panels. SUBSTANCE: phosphor layer is formed in vacuum while exciting vertical vibrations at frequency of 2-3 Hz for two or three minutes. EFFECT: enhanced brightness, stability, and electric strength. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHODS FOR MANUFACTURING OF ELECTROLUMINESCENT LIGHT SOURCE | 1992 |
|
RU2050041C1 |
METHOD FOR MANUFACTURING ELECTRIC LUMINESCENT LIGHT SOURCE | 2003 |
|
RU2253951C2 |
METHOD FOR MANUFACTURING OF ELECTROLUMINESCENT LIGHT SOURCES AND DEVICE FOR ITS IMPLEMENTATION | 1992 |
|
RU2050042C1 |
ELECTROLUMINESCENT LIGHT SOURCE | 2007 |
|
RU2350050C2 |
ELECTROLUMINESCENT FLEXIBLE SOURCE OF MINI-NEON LIGHT | 2016 |
|
RU2624915C1 |
METHOD OF TESTING ELECTROLUMINOPHOR FOR STABILITY | 0 |
|
SU1770856A1 |
METHOD OF MANUFACTURING ELECTROLUMINESCENT SCREEN | 0 |
|
SU690660A1 |
PROCESS OF MANUFACTURE OF ELECTROLUMINESCENT SIGN INDICATOR WITH ALTERING COLOR OF GLOW | 1991 |
|
RU2012949C1 |
EXHIBIT IDENTIFICATION SYSTEM | 2009 |
|
RU2419887C2 |
DEVICE TO EXCITE ELECTROLUMINESCENCE | 2007 |
|
RU2350049C1 |
Authors
Dates
2001-04-20—Published
1999-06-15—Filed