FIELD: methods and devices for aerodynamic texturing of continuous threads. SUBSTANCE: invention is based on use of texturing nozzle according to WO97/30200 and striving to considerably exceed double M number. Said invention also provides for heat treatment before and/or after texturing. In process of treatment, air pressure rises up to 10-14 bars and above. EFFECT: higher increase of production efficiency in aerodynamic texturing in interval of 800-1500 m/min and above with invariable high quality due to combination of thread heat treatment, higher pressure and intensive texturing. 10 cl, 13 dwg