FIELD: ferrous metallurgy; iron smelting. SUBSTANCE: proposed method includes loading iron ore charge containing pellets at basicity of 0.3 to 0.5 and sinter cake. Use is made of sinter cake containing titanium and magnetite alumina concentrate, quartzitic concentrate and ore at the following percentage: first concentrate, 20 to 25; second concentrate, 40 to 50 and ore, 30 to 40. This sinter cake is used together with 30-70% pellets to ensure obtaining charge in blast furnace at basicity of B= (CaO+MgO)/(SiO2+Al2O3) within 1.03 and 1.07 at ratio B/ma.m.m. within 1 and 1.04 and ratio of content of MgO in slag to titanium in cast iron ranges from 230 to 270. EFFECT: possibility of production of low-sulfur iron at low consumption of coke and increased furnace output. 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF BLAST-FURNACE SMELTING | 2000 |
|
RU2177039C1 |
METHOD OF BLAST-FURNACE SMELTING | 2000 |
|
RU2172780C1 |
METHOD OF BLAST-FURNACE SMELTING | 1999 |
|
RU2150510C1 |
PROCEDURE FOR BLAST MELTING TITANIUM-MAGNETITE RAW MATERIAL | 2008 |
|
RU2385352C2 |
METHOD OF CONVERSION PIG IRON SMELTING IN BLAST FURNACE | 1995 |
|
RU2096475C1 |
PROCEDURE FOR METALLISATION OF TITANIUM-MAGNESIUM CONCENTRATES AT PRODUCTION OF IRON PELLETS AND TITANIUM-VANADIUM SLAG | 2008 |
|
RU2399680C2 |
BLAST-FURNACE MELTING METHOD OF TITANIUM-BEARING IRON-ORE RAW MATERIALS | 2007 |
|
RU2351657C2 |
IRON FLUX CONTAINING VANADIUM | 2009 |
|
RU2419658C2 |
METHOD OF BLAST-FURNACE HEAT RUNNING | 1999 |
|
RU2156306C1 |
METHOD OF BLAST-FURNACE SMELTING OF TITANOMAGNETITE ORES | 2001 |
|
RU2210598C2 |
Authors
Dates
2002-01-10—Published
2000-06-27—Filed