FIELD: welding technology. SUBSTANCE: fusing agent contains, wt %: alumina 20-25, calcium oxide 5-8, mixed zirconium and hafnium oxyfluoride 2-5, and calcium fluoride - the balance. Sources of calcium fluoride and zirconium and hafnium oxyfluorides utilized are leaching products of zircon cake, potassium silicofluoride, and potassium chloride. Microalloying and modifying metal to increase corrosion and mechanical properties thereof is also possible. EFFECT: improved quality of surface of welded metal and high-temperature conductance stability of fusing agent. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
FLUX FOR AUTOMATIC HARD-FACING BY TAPE ELECTRODE | 2013 |
|
RU2526623C1 |
WELDING FLUX | 2001 |
|
RU2207237C2 |
FLUX FOR WELDING AND SURFACING | 1994 |
|
RU2074800C1 |
PROCEDURE FOR MELTING HOLLOW INGOTS OF TITAN AND BORON CONTAINING GRADES OF STEEL BY METHOD OF ESR (ELECTRO-SLAG RE-MELTING) | 2009 |
|
RU2423536C1 |
WELDING FLUX | 1995 |
|
RU2080227C1 |
CERAMIC FLUX FOR AUTOMATIC WELDING AND DEPOSIT WELDING | 2012 |
|
RU2493945C1 |
MINERAL ALLOY FOR WELDING ELECTRODE COATINGS | 2012 |
|
RU2497646C1 |
AGGLOMERATED FLUX FOR WELDING AND SURFACING WITH STAINLESS STEELS | 2018 |
|
RU2688021C1 |
FLUX FOR MELT, REFINING, INOCULATION OF NON-FERROUS METALS AMD ALLOYS | 2003 |
|
RU2230809C1 |
WELDING FLUX | 2001 |
|
RU2203787C2 |
Authors
Dates
2002-02-20—Published
2000-09-19—Filed