FIELD: precious metal technology. SUBSTANCE: palladium is extracted with sulfide-containing extractant and then reextracted with ammonium chloride/sodium carbonate mixture (10-214 and 10-100 g/l, respectively). Contacting time during reextraction varies between 5 and 30 min and ratio of organic to aqueous phases is 1:(0.1-3). EFFECT: enabled recovery of palladium both from sulfide and from sulfoxide extractants, reduced phase separation time. 3 cl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF EXTRACTION OF PALLADIUM | 2000 |
|
RU2161129C1 |
METHOD OF RECOVERING AND SEPARATING PLATINUM AND PALLADIUM | 1998 |
|
RU2121517C1 |
METHOD OF RECOVERING AND SEPARATING PLATINUM-GROUP METALS | 2002 |
|
RU2200132C1 |
METHOD OF RECOVERING AND PURIFYING PLATINUM GROUP METALS AND GOLD | 1997 |
|
RU2108294C1 |
METHOD OF RECOVERING PALLADIUM FROM HYDROCHLORIC ACID SOLUTION | 1998 |
|
RU2130429C1 |
METHOD OF RECOVERY AND SEPARATION OF PLATINUM GROUP METALS | 2000 |
|
RU2161130C1 |
METHOD OF PREPARING PLATINUM GROUP METALS FROM TIN- CONTAINING SOLUTION | 1999 |
|
RU2156818C1 |
METHOD FOR RECOVERING METALS | 0 |
|
SU954466A1 |
METHOD OF PURIFYING RHODIUM AND IRIDIUM | 1999 |
|
RU2156819C1 |
METHOD FOR COLUMBITE CONCENTRATE PROCESSING | 2014 |
|
RU2576562C1 |
Authors
Dates
2003-03-10—Published
2002-03-15—Filed