FIELD: inorganic synthesis catalysts. SUBSTANCE: catalyst used for decomposing ozone is prepared by mixing exhausted carbon monoxide oxidation catalyst based on manganese dioxide, copper oxide, and bentonite clay (binding agent) with water and keeping mixture in water during 40 to 150 h followed by granulation, drying, crushing, and heat treatment. EFFECT: considerable increased strength of catalyst. 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF CATALYST FOR OZONE DECOMPOSITION | 2002 |
|
RU2218211C1 |
CATALYST PREPARATION PROCESS | 2001 |
|
RU2193923C1 |
METHOD OF PREPARING CARBON MONOXIDE OXIDATION CATALYST | 1997 |
|
RU2129914C1 |
METHOD OF PREPARING CATALYST FOR CARBON OXIDE OXIDATION | 1993 |
|
RU2054322C1 |
METHOD OF PREPARING CARBON MONOXIDE OXIDATION CATALYST | 1997 |
|
RU2119387C1 |
METHOD OF MANUFACTURE OF CERAMIC ARTICLES | 2000 |
|
RU2185350C2 |
METHOD OF PREPARING CATALYST FOR CARBON MONOXIDE OXIDATION | 1995 |
|
RU2083279C1 |
METHOD OF PREPARING CATALYST FOR CARBON MONOXIDE OXIDATION | 1996 |
|
RU2103067C1 |
METHOD OF PREPARING CARBON MONOXIDE OXIDATION CATALYST | 1997 |
|
RU2120335C1 |
METHOD OF PREPARING LOW-TEMPERATURE CARBON MONOXIDE OXIDATION CATALYST | 1997 |
|
RU2116833C1 |
Authors
Dates
2003-10-10—Published
2002-05-28—Filed