FIELD: varnish-and-paint industry. SUBSTANCE: silicate enamel suitable for coating architectural articles and household dishes contains, wt %: P2O5 31.93-32.7, Al2O3 24.17-24.76, B2O3 10.94-11.20, K2O 3.41-3.50, Na2O 21.34-23.21, and TiO2 6.34-6.50. Firing temperature of enamel is 550 C, firing temperature interval 540-570 C, brilliance 65%, temperature resistance 20-250-20 C is 2-3 cycles, and adhesion force 72%. EFFECT: lowered firing temperature and prolonged lifetime due to increased chemical resistance of glass-enamel coating. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
DROSS FOR HEAT-RESISTANT DEVITRIFIED GLASS COVER PRODUCING | 2000 |
|
RU2183598C2 |
ONE-LAYER LOW-MELTING ENAMEL FOR STREET | 1998 |
|
RU2141458C1 |
STEEL LINING | 2001 |
|
RU2230712C2 |
FRIT FOR COLOURED MONOLAYER ENAMEL | 2007 |
|
RU2345964C2 |
FRIT FOR SINGLE LAYER ENAMEL COATING | 2003 |
|
RU2247084C1 |
PROTECTIVE GLASSCERAMIC COATING FOR STEEL | 2010 |
|
RU2453512C1 |
INSULATING ENAMEL | 2001 |
|
RU2209786C2 |
ELECTROINSULATING ENAMEL FOR STAINLESS STEEL PARTS | 1999 |
|
RU2203233C2 |
METHOD FOR STEEL TREATMENT BEFORE ENAMEL COATING | 2003 |
|
RU2248410C1 |
HEAT-RESISTANT GLASS-CERAMIC COVER WITH DEVITRIFIED GLASS STRUCTURE FOR NICHROME STEEL AND ALLOY | 2004 |
|
RU2275341C1 |
Authors
Dates
2003-10-10—Published
2001-12-13—Filed