FIELD: rocket fuels.
SUBSTANCE: method comprises formation of charge at temperature of fuel body by 10-20оС below curing temperature and curing under pressure. Press mold, prior to be filled, is heated for 0.5 to 12 h at temperature by 5-10оС superior to molding temperature and charge is then formed in press mold heated with air supplied under casing or flexible jacket of press mold at temperature by 10оС superior to molding temperature.
EFFECT: improved quality of charge regarding its solidity and equilibrium temperature, and excluded undesired pressure surge during curing.
2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING CHARGE OF MIXED SOLID ROCKET FUEL | 2002 |
|
RU2230722C2 |
A METHOD OF DEFINITION OF AN EQUILIBRIUM TEMPERATURE OF A MIXED ROCKET SOLID PROPELLANT CHARGE | 2002 |
|
RU2227131C1 |
PROCESS OF MANUFACTURE OF CHARGES OF BLENDED SOLID ROCKET FUEL | 2000 |
|
RU2198153C2 |
METHOD TO MANUFACTURE A CHARGE OF ROCKET SOLID PROPELLANT MIXTURE | 2002 |
|
RU2220935C1 |
METHOD OF MANUFACTURING CHARGES OF SOLID MIXED ROCKET FUEL | 2000 |
|
RU2179543C2 |
METHOD OF PREPARING CHARGES OF MIXED SOLID ROCKET FUEL | 1999 |
|
RU2196760C2 |
METHOD TO MANUFACTURE A CHARGE OF MIXED SOLID PROPELLANT FOR ROCKETS | 2002 |
|
RU2219150C2 |
METHOD OF PREPARING CHARGE OF BLENDED ROCKET SOLID FUEL | 2003 |
|
RU2238254C1 |
METHOD OF PREPARING CHARGE FOR BLENDED SOLID ROCKET FUEL | 2002 |
|
RU2240298C2 |
METHOD FOR MANUFACTURING OF ITEM FROM MIX SOLID ROCKET PROPELLANT | 2008 |
|
RU2382017C1 |
Authors
Dates
2004-11-10—Published
2003-02-26—Filed