FIELD: explosives.
SUBSTANCE: method for manufacturing of item from mix rocket solid propellant (MRSP) includes moulding of item, execution of staged hardening of item under pressure by means of coolant temperature variation and item cooling. Item is hardened at initial stage at the temperature of coolant 5-15°C below temperature of the main hardening mode for 10-20% of overall hardening duration, and then in the main mode at the temperature of 60 - 80°C. Cooling is carried out at coolant temperature of 10 - 35°C and duration (τcooling, hr), defined by formula τcooling=0.61 Taverage + 0.65, where Taverage is actual average coolant temperature, °C.
EFFECT: invention makes it possible to reduce duration of item cooling process.
1 dwg, 1 tbl, 12 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING CHARGE OF MIXED SOLID ROCKET FUEL | 2002 |
|
RU2230722C2 |
METHOD FOR DETERMINATION OF EQUILIBRIUM TEMPERATURE OF MIX SOLID PROPELLANT ITEM FIXED TO CASING IN PROCESS OF ITS MANUFACTURE | 2007 |
|
RU2352548C1 |
METHOD OF PRODUCING COMPOSITE SOLID PROPELLANT | 2009 |
|
RU2413708C1 |
METHOD OF MAKING ARTICLES FROM MIXED SOLID ROCKET FUEL | 2009 |
|
RU2394011C1 |
METHOD OF PRODUCTION OF THE ROCKET SOLID PROPELLANT CHARGE | 2005 |
|
RU2280632C1 |
METHOD OF PRODUCING MIXED SOLID-PROPELLANT ROCKET ARTICLE | 2010 |
|
RU2434830C1 |
METHOD OF PRODUCING MIXED ROCKET SOLID PROPELLANT PRODUCT | 2007 |
|
RU2361850C1 |
METHOD TO PRODUCE COMPOSITE SOLID PROPELLANT | 2009 |
|
RU2407728C1 |
METHOD OF PREPARING CHARGE OF BLENDED SOLID ROCKET FUEL | 2003 |
|
RU2239621C1 |
METHOD OF MANUFACTURING CHARGES OF SOLID MIXED ROCKET FUEL | 2000 |
|
RU2179543C2 |
Authors
Dates
2010-02-20—Published
2008-08-18—Filed