FIELD: metallurgy, in particular complex alloy for deoxidation and doping of steel and cast iron.
SUBSTANCE: claimed addition alloy contains (mass %): iron 25-50; aluminum and silicium 75-50 in Al/Si ratio of (1:1)-(3:2). Claimed Al/Si ratio is the most preferable to produce high quality ingots due to more deep steel deoxidation with aluminum and sufficient steel doping with silicium.
EFFECT: increased coefficient of aluminum utilization; method for producing of silicon steel with improved efficiency.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SMELTING OF FERROALUMINUM | 2003 |
|
RU2241777C1 |
STEEL DEOXIDATION AND REFINING BRIQUETTE | 2002 |
|
RU2226556C1 |
FLUX FOR REDUCING, REFINING, MODIFYING AND ALLOYING STEEL | 2009 |
|
RU2396364C1 |
EXOTHERMIC MIXTURE FOR STEEL DEOXIDATION, REFINING, INOCULATION AND ALLOYING | 2004 |
|
RU2252265C1 |
METHOD OF MANUFACTURING VANADIUM-MICROALLOYED STEEL | 1997 |
|
RU2118380C1 |
METHOD OF OBTAINING IRON-CARBON ALLOYS IN METALLURGICAL UNITS OF VARIOUS FUNCTIONAL PURPOSE | 2018 |
|
RU2688015C1 |
CAKE FOR A STEEL DEOXIDATION | 2004 |
|
RU2259405C1 |
ACTIVE DEOXIDIZER OF LIQUID AND REFRACTORY HOT AND COLD SLAGS | 2022 |
|
RU2786789C1 |
METHOD OF OUT-OF-FURNACE TREATMENT OF STEEL IN LADLE | 2020 |
|
RU2735697C1 |
METHOD FOR DEOXIDATION AND ALLOYING OF METAL MELTS | 2005 |
|
RU2319751C2 |
Authors
Dates
2004-12-10—Published
2003-05-21—Filed