FIELD: building materials, in particular protective and ornamental facing of concrete and daubed surfaces.
SUBSTANCE: claimed mixture contains (mass %): iron sulfate 28-35; liquid glass 13-20; filler (e.g., waste from neutralization of polishing fluid from glass manufacturing) 32-40; and water 14-18.
EFFECT: nonshrinking building mixture with high cohesive resistance and reduced time of desiccation.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
SPACKLING COMPOUND | 2004 |
|
RU2281269C2 |
COMPOSITION FOR BUILDING ARTICLE MAKING | 2000 |
|
RU2182567C1 |
METHOD FOR PRODUCING GYPSUM BINDER WITH SELF-CLEANING PROPERTIES FROM TITANIUM DIOXIDE PRODUCTION WASTE | 2023 |
|
RU2812750C1 |
RAW MIX FOR PRODUCTION OF NON-SHRINK CONSTRUCTION MATERIAL | 2007 |
|
RU2352537C1 |
SEALING PASTE | 2004 |
|
RU2274619C2 |
COMPOSITION FOR THE MANUFACTURE OF WATERPROOF FACING GYPSUM PRODUCTS | 2022 |
|
RU2787245C1 |
MIXTURE FOR FINISHING WORKS | 2003 |
|
RU2252204C2 |
COMPOSITION FOR FIBROUS HEAT- AND SOUND-INSULATION MATERIAL AND METHOD OF MANUFACTURING THEREOF | 1997 |
|
RU2125029C1 |
UNDERPAINT PUTTY | 0 |
|
SU1174408A1 |
FACADE DECORATIVE COMPOSITE MATERIAL | 2016 |
|
RU2625059C1 |
Authors
Dates
2005-03-20—Published
2003-02-14—Filed