FIELD: manufacture of building materials.
SUBSTANCE: powdered mixture of glass, carbonate gasifier, and chemically active substance (0.8-5%) is heated in metal mold with adjustable walls and removable liner placed in oven. Heating is carried out until foaming temperature (680-740°C) for 0.8-1.5 h. resulting foamed glass blocks are then placed in annealing chamber, wherein cooling from 600°C to 50°C is accomplished at cooling velocity 1.2-1.6°C/min.
EFFECT: reduced foaming temperature.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING FOAMED GLASS | 2010 |
|
RU2459769C2 |
RAW MIX FOR MANUFACTURING OF BLOCK FOAM GLASS AND METHOD OF ITS MANUFACTURING | 2014 |
|
RU2570175C1 |
BLEND FOR PREPARING FOAM GLASS | 1998 |
|
RU2149146C1 |
METHOD FOR PRODUCTION OF FOAM GLASS | 2008 |
|
RU2351554C1 |
METHOD FOR PRODUCTION OF THERMAL INSULATION BOARDS FROM FOAM GLASS BASED ON CULLET | 2022 |
|
RU2781293C1 |
CHARGE COMPOSITION FOR PRODUCING HEAT-INSULATING BLOCKS FROM NATURAL QUARTZ SAND | 2023 |
|
RU2817428C1 |
CHARGE COMPOSITION FOR PRODUCING HEAT-INSULATING BLOCKS FROM APATITO-NEPHELINE ORES PROCESSING WASTE | 2022 |
|
RU2799217C1 |
PRODUCTION OF BLOCK HEAT-RESISTANT FOAM GLASS | 2013 |
|
RU2530151C1 |
COMPOSITION OF FOAMED GLASS COMPOSITE | 2015 |
|
RU2592002C1 |
FOAMING MIXTURE AND A METHOD OF PRODUCTION OF A MODULAR FOAMED GLASS WITH THE MIXTURE USE | 2003 |
|
RU2265582C2 |
Authors
Dates
2006-12-27—Published
2005-07-11—Filed