FIELD: application of coats by gas dynamic methods.
SUBSTANCE: first flux is applied on surface of part at activity time of 0.2-0.25 h which contains up to 30% of ammonium chloride NH4Cl, up to 70% of zinc chloride ZnCl2 and up to 2% of potassium permanganate KMnO4. Then, surface is heated over flux with the aid of torch producing oxidizing flame to temperature of (0.14-0.2)Tml., where Tml. is cast iron melting point. Then, part is treated with abrasive powder at size of particles of 30-300 mcm. Compressed air is heated and is fed to supersonic nozzle where supersonic air flow is formed; powder material for forming the coat is fed to this air flow in the direction of surface of article to be coated.
EFFECT: enhanced adhesion strength of coat on cast iron articles.
2 dwg, 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD TO APPLY COATINGS | 2010 |
|
RU2450087C2 |
METHOD OF REDUCING TITANIUM PARTS | 2019 |
|
RU2742861C2 |
COATING METHOD | 2001 |
|
RU2205897C1 |
METHOD OF GAS-DYNAMIC SPUTTERING OF ANTICORROSION COATING FROM A CORROSION-RESISTANT COMPOSITION ONTO THE SURFACE OF CONTAINER FOR TRANSPORTING AND/OR STORING SPENT NUCLEAR FUEL, MADE FROM HIGH-STRENGTH IRON WITH GLOBULAR GRAPHITE | 2014 |
|
RU2593041C2 |
MANUFACTURING METHOD OF FUNCTIONAL SURFACE | 2007 |
|
RU2353706C2 |
METHOD OF RESTORATION OF ART WORKS AND THEIR ELEMENTS MADE OF FERROUS METAL | 2017 |
|
RU2699691C2 |
COATING METHOD | 1990 |
|
RU2102528C1 |
METHOD FOR MANUFACTURING OF ANTIFRICTION RECOVERY COATING AT STEEL PRODUCT (VERSIONS) | 2012 |
|
RU2532653C2 |
METHOD FOR SPUTTERING OF COATING TO PRODUCT FROM NATURAL STONE OR FROM METAL MATERIAL, AND DEVICE FOR ITS IMPLEMENTATION | 2011 |
|
RU2489519C2 |
POWDER MATERIAL FOR GAS-DYNAMIC SPUTTERING OF DEFECT HEADS OF CYLINDER BLOCKS | 2018 |
|
RU2688025C1 |