FIELD: CHEMISTRY.
SUBSTANCE: method for preparation of low-basic anionites by suspension copolymerisation of acrylonitrile, methylmethacrylate in amount of З-5 wt.%, content of technical grade divinylbenzene being 9-15 wt.% and concentration thereof being 50-60%, in the presence of benzoperoxide in amount of 3.0 wt.% and blowing agent (alkylbenzine, aviation kerosene, decane) in amount of 40 vol.% as regards to monomer volume in suspension media, which consists of water, 25% of sodium chloride or ammonium chloride and 1.5-2.0% of potato starch, when heated at 50°С for 1 hour, at 61-65°С for 4 hours, at 70°С for 2 hours, at 80°С for 1 hour, followed by amination with diethylenetriamine at 130-145°С for 10 hours in the presence of 1.0-1.5% of element sulphur used as a catalyst.
EFFECT: provides for high osmotic stability and high resistance to organic poisoning.
1 cl, 9 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING CARBOXYLIC CATION EXCHANGE RESIN | 2006 |
|
RU2326130C1 |
PROCESS FOR PREPARING LOW-BASIC ANIONITES | 1995 |
|
RU2080338C1 |
METHOD FOR SYNTHESIS OF POROUS WEAKLY BASIC ANIONITES | 2008 |
|
RU2387673C1 |
METHOD OF PRODUCING EASILY REGENERATED IONITE | 2012 |
|
RU2493915C1 |
METHOD OF OBTAINING CARBOXYLIC CATIONITES | 2008 |
|
RU2391356C1 |
PROCESS FOR PREPARING ANIONITES | 1997 |
|
RU2127283C1 |
ANIONITE FOR EXTRACTION OF URANIUM AND METHOD OF PRODUCTION THEREOF | 2023 |
|
RU2820543C1 |
METHOD FOR OBTAINING ANIONITES | 0 |
|
SU1657513A1 |
METHOD FOR ION EXCHANGER PREPARATION FOR GOLD SORPTION | 2016 |
|
RU2615522C1 |
METHOD OF OBTAINING LOW-BASIC ARTICLES | 0 |
|
SU1571050A1 |
Authors
Dates
2008-05-10—Published
2006-09-21—Filed