FIELD: technological processes.
SUBSTANCE: initial substance 2 is heated by exothermal reaction of termite mixture 3 combustion, which contains catalyst, exposed to shock pressure created with blasting charge 5, and cooled on separate metal surface, which is made in the form of tube 1. Blasting charge 5 is installed around tube 1. Initial substance 2 is used in the form of geometric reflection of tubular cavity, and thermite mixture 3 is placed around it. Impact of shock pressure is carried out after heating of initial substance, its displacement into tubular cavity and its filling.
EFFECT: increase of diamonds output and reduction of power inputs and blasting charge consumption.
2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DIAMOND OR CUBIC BORON NITRIDE SYNTHESIS | 2000 |
|
RU2199380C2 |
METHOD OF SYNTHESIZING DIAMOND | 2001 |
|
RU2259943C2 |
LIQUID FORMING METHOD | 1999 |
|
RU2198065C2 |
METHOD OF AUTOCLAVE PRODUCTION OF CHEMICALLY ACTIVE MATERIALS AND DEVICE TO THIS END | 2008 |
|
RU2405045C2 |
PROCEDURE BY VOLKOV FOR PRODUCTION OF CHEMICALLY ACTIVE METALS AND DEVICE FOR IMPLEMENTATION OF THIS PROCEDURE | 2008 |
|
RU2401874C2 |
METHOD AND DEVICE FOR LIQUID FORGING OF DOUBLE ACTION | 2018 |
|
RU2764620C2 |
PROCEDURE FOR PRODUCTION OF CHEMICALLY ACTIVE METALS AND REDUCTION OF SLAG AND DEVICE FOR IMPLEMENTATION OF THIS METHOD | 2008 |
|
RU2401875C2 |
METHOD OF PREPARING DIAMOND IN DETONATION WAVE | 1994 |
|
RU2100063C1 |
METHOD OF OBTAINING OF CUBIC SILICON NITRIDE | 2006 |
|
RU2331578C2 |
METHOD AND DEVICE FOR PULSE CLOSE-DIE FORGING OF METALS BY INDUCTION MELT RETENTION | 2011 |
|
RU2555278C2 |
Authors
Dates
2008-10-10—Published
2003-06-09—Filed