FIELD: chemistry.
SUBSTANCE: crude mixture for moulding granules is prepared by mixing kaolin with powdered zeolite A, metakaolin and starch. Metakaolin is first obtained by annealing kaolin at temperature 500-850°C for 1-8 hours. The mixture of components is moistened, mixed and granules are moulded. The granules are dried, annealed and crystallised, washed and dried.
EFFECT: obtained granular zeolite A which does not contain binder has high mechanical strength and packed density.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING NAA GRANULATED ZEOLITE ADSORBENT | 2017 |
|
RU2655104C1 |
METHOD OF PRODUCING HIGH PHASE PURITY ZEOLITE ADSORBENT OF STRUCTURE A AND X, GRANULATED WITHOUT BINDER | 2009 |
|
RU2420457C1 |
METHOD OF PRODUCING HIGH PHASE PURITY ZEOLITE A GRANULATED WITHOUT BINDER | 2009 |
|
RU2420456C1 |
METHOD OF PREPARING HIGH PHASE-PURITY GRANULATED A-TYPE ZEOLITE | 2005 |
|
RU2283281C1 |
METHOD OF OBTAINING GRANULATED WITHOUT BINDING AGENT NaY TYPE ZEOLITE WITH HIGH PHASE PURITY | 2014 |
|
RU2568219C1 |
METHOD OF PREPARING SYNTHETIC A-TYPE ZEOLITE | 2005 |
|
RU2283280C1 |
METHOD OF PRODUCING HIGH PHASE PURITY GRANULAR NaY ZEOLITE WITHOUT BINDER | 2009 |
|
RU2412903C1 |
METHOD OF OBTAINING HIGH-PHASE PURITY GRANULAR NaX ZEOLITE WITHOUT BINDER | 2009 |
|
RU2404122C1 |
METHOD OF PRODUCING HIGH-MODULUS FAUJASITE WITHOUT BINDING MATERIALS | 2010 |
|
RU2456238C1 |
METHOD FOR PRODUCING GRANULATED ZEOLITE TYPE X WITHOUT BINDERS | 2017 |
|
RU2653033C1 |
Authors
Dates
2011-08-10—Published
2009-10-22—Filed