FIELD: construction.
SUBSTANCE: mixture for autoclave foam concrete, including portland cement, quicklime lime, sand in the form of sand slurry with a density of about 1.6 g/l, obtained by wet grinding to a specific surface of particles of 280-300 m2/kg, foam-based protein-based additive, water and waste-condensate, formed during the autoclave processing of the cut foam concrete massif, additionally contains muscovite, co-grinded with sand wet grinding, ferrous sulfate, at the following ratio of components, wt %: Portland cement 17.00-19.38, mentioned muscovite 1.75-1.95, ferrous sulfate 0.52-0.59, mentioned lime 6.9-7.18, mentioned sand 43.42-45.03, mentioned foaming agent 0.23-0.24, water 19.46-19.61, mentioned waste-condensate 8.34-8.40.
EFFECT: increase in the coefficient of vapor permeability and decrease in the coefficient of thermal conductivity of finished products.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
AUTOCLAVE FOAM CONCRETE MIXTURE | 2009 |
|
RU2403232C1 |
MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2011 |
|
RU2484066C1 |
MIXTURE FOR AUTOCLAVE FOAMED CONCRETE | 2016 |
|
RU2625063C1 |
AUTOCLAVE FOAMED CONCRETE MIXTURE | 2009 |
|
RU2394795C1 |
AUTOCLAVE FOAM-ASH CONCRETE | 2009 |
|
RU2395478C1 |
MIXTURE FOR MAKING AUTOCLAVE FOAM CONCRETE | 2011 |
|
RU2491258C2 |
RAW MATERIAL MIX FOR AUTOCLAVE FOAM CONCRETE | 2007 |
|
RU2354630C1 |
MIXTURE FOR PRODUCING AUTOCLAVED CELLULAR CONCRETE | 2011 |
|
RU2477716C1 |
RAW MATERIAL MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2013 |
|
RU2542011C1 |
STEAM CURED FOAMED CONCRETE | 2004 |
|
RU2255074C1 |
Authors
Dates
2017-07-11—Published
2016-06-29—Filed