FIELD: chemistry.
SUBSTANCE: cryolite is obtained by mixing aluminium oxide, sodium chloride and ammonium hydrodifluoride or fluoride in stoichiometric ratio, taken in excess of up to 20% of the stoichiometric ratio. The obtained mixture is heated at the first stage to 240°C and kept at this temperature until complete separation of ammonia gas and water, and at the second stage - to 400°C and kept until complete subliminal removal of ammonium chloride.
EFFECT: invention allows for obtaining cryolite and ammonium chloride at the same time.
2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING SODIUM HYDROFLUORIDE | 2009 |
|
RU2415810C1 |
METHOD FOR PRODUCING SYNTHETIC SILICON DIOXIDE OF HIGH PURITY | 2020 |
|
RU2747934C1 |
METHOD OF PRODUCING ALUMINIUM FLUORIDE | 2009 |
|
RU2421401C1 |
METHOD OF PRODUCING HIGH-PURITY SYNTHETIC SILICON DIOXIDE | 2010 |
|
RU2458006C2 |
METHOD OF PRODUCING SYNTHETIC SILICON DIOXIDE | 2015 |
|
RU2600640C1 |
SILICON DIOXIDE PROCESS | 2007 |
|
RU2357925C1 |
METHOD OF EXTRACTING OXIDES OF RARE EARTH ELEMENTS OUT OF GRINDING WASTES OF CONSTANT MAGNET PRODUCTION | 2008 |
|
RU2369561C1 |
0 |
|
SU392000A1 | |
METHOD OF PROCESSING OF RAW MATERIALS CONTAINING TITANIUM | 2008 |
|
RU2365647C1 |
METHOD OF PRODUCING LITHIUM HEXAFLUOROPHOSPHATE | 2009 |
|
RU2421396C1 |
Authors
Dates
2009-07-20—Published
2008-01-23—Filed