FIELD: metallurgy.
SUBSTANCE: ligature according to the first option of invention contains magnesium, wt %: calcium 0.1-6, rare-earth metals 0.2-10, aluminium 2-40, vanadium 0.1-14, titanium 0.1-1, magnesium 0.5-12, iron is the rest. Ligature according to the second option contains, wt %: calcium 0.1-6, rare-earth metals 0.2-10, aluminium 2-40, vanadium 0.1-14, titanium 0.1-1, magnesium 0.5-12, one or several elements from group containing niobium, zirconium, barium, and not exceeding 3, iron - the rest.
EFFECT: increasing of fixation degree of active components by melt, decrease in value of ligature, improvement of metal and improvement of ecological environment on working station.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
HARDENER (VERSIONS) | 2001 |
|
RU2191213C1 |
CAST IRON | 0 |
|
SU1439145A1 |
STEEL MODIFIER | 2002 |
|
RU2228384C1 |
MASTER ALLOY FOR REDUCING AND ALLOYING STEEL | 0 |
|
SU1089161A1 |
STEEL AND CAST IRON ADDITIVE (OPTIONS) | 2003 |
|
RU2239669C1 |
MODIFIER | 0 |
|
SU1724715A1 |
ALLOY BASED ON IRON-CARBON SYSTEM FOR CASTING OF WEAR-RESISTANCE ARTICLES AND METHOD OF ALLOY PRODUCTION | 1997 |
|
RU2109837C1 |
MATERIAL FOR STEEL REFINING | 2003 |
|
RU2245390C1 |
MATERIAL FOR MICROALLOYING USING A FURNACE-LADLE INSTALLATION | 2002 |
|
RU2238983C2 |
MODIFIER | 0 |
|
SU960295A1 |
Authors
Dates
2009-07-20—Published
2008-03-14—Filed