FIELD: chemistry.
SUBSTANCE: invention can be used for producing hydrated material for reducing content of SO2 in waste gases. In the method of hydrating CaO containing material in form of particles or powder, water is added in an amount sufficient for maintaining partial pressure PH2O, as a function of temperature, within a range defined by the formula where PH2O - is partial pressure of water vapour in atm, and T - is temperature in °C. Temperature in the hydration process is kept above 200°C, and partial pressure of water vapour ranging from 0.9 to 1.1 atm. A device is proposed for realising the said method, the obtained product and use of that product.
EFFECT: reduced agglomeration of particles and increased uniformity of their hydration.
13 cl, 4 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD AND INSTALLATION FOR CEMENT CLINKER PRODUCTION | 2009 |
|
RU2535855C2 |
METHOD OF REDUCTION OF EMISSION OF SO FROM PLANT PRODUCING CEMENT CLINKER AND CEMENT CLINKER PLANT FOR REALIZATION OF THIS METHOD | 2001 |
|
RU2259226C2 |
METHOD TO PRODUCE PORTLAND CEMENT CLINKER | 2013 |
|
RU2525555C1 |
METHOD AND INSTALLATION FOR PRODUCTION OF CEMENT CLINKER | 2007 |
|
RU2387606C1 |
METHOD OF TEMPERATURE CONTROL IN KILN AND DEVICE FOR PRODUCTION OF CEMENT CLINKER | 1995 |
|
RU2136622C1 |
METHOD AND PLANT FOR PRODUCTION OF CEMENT CLINKER | 2003 |
|
RU2315736C2 |
METHOD AND DEVICE FOR HEATING POWDERED OR DUST-LIKE MATERIAL | 2004 |
|
RU2349559C2 |
PRODUCTION OF PORTLAND CEMENT CLINKER (VERSIONS) | 2013 |
|
RU2547195C1 |
METHOD TO PRODUCE PORTLAND CEMENT CLINKER (VERSIONS) | 2014 |
|
RU2574795C1 |
APPARATUS FOR BURNING CEMENT CLINKER | 0 |
|
SU805037A1 |
Authors
Dates
2009-10-20—Published
2005-02-16—Filed