FIELD: chemistry.
SUBSTANCE: method is suggested for production of beta-sialon, in which thermal treatment of mixture of aluminium powder with specific surface area equal to 22.0-24.0 m2/g, and crystalline silicon powder with specific surface area of 0.2-0.3 m2/g, taken in the ratio of 1:1, is carried out by heating up to temperature of 1100-1200°C with heating rate of 10-12°/minute in air atmosphere.
EFFECT: method simplification at high yield of finished product.
2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING ULTRAFINE BETA-SIALON POWDER | 2009 |
|
RU2421428C2 |
β-SIALON PRODUCING METHOD | 1986 |
|
SU1522704A1 |
METHOD OF PREPARING OF SIALONE POWDER | 1990 |
|
RU1774612C |
β′ SIALON POWDER PRODUCTION METHOD | 1989 |
|
SU1626601A1 |
METHOD FOR PRODUCING COATINGS FROM BORON NITRIDE NANOSHEETS | 2016 |
|
RU2613996C1 |
CERAMIC COMPOSITE BASED ON SIALON AND METHOD FOR MANUFACTURING ARTICLES | 2006 |
|
RU2329997C2 |
METHOD OF PREPARING SIALON POWDER | 2008 |
|
RU2378227C1 |
METHOD FOR PRODUCING SIALON CERAMICS USING PLASMA ENERGY | 2021 |
|
RU2798804C2 |
METHOD FOR PREPARING BETA-SIALONE POWDER | 2003 |
|
RU2261848C2 |
METHOD FOR PRODUCING NANOPOROUS BORON NITRIDE | 2016 |
|
RU2614007C1 |
Authors
Dates
2010-03-20—Published
2008-05-04—Filed