FIELD: chemical technology.
SUBSTANCE: method for preparing β-sialone powder by carbothermal reduction of kaolin involves thermal treatment of charge in nitrogen atmosphere at 1710-1780°C for 5-25 min. Charge comprises a carbon component with particles size 20-500 nm. An average size of particles of prepared β-sialone powder can be regulated by using the disperse carbon component of charge with the required size of particles. Invention provides the development of rapid and simple in realization method for preparing β-sialone powder providing preparing β-sialone with the required size of particles.
EFFECT: improved preparing method.
2 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING ULTRAFINE BETA-SIALON POWDER | 2009 |
|
RU2421428C2 |
METHOD FOR PRODUCING SIALON CERAMICS USING PLASMA ENERGY | 2021 |
|
RU2798804C2 |
MANUFACTURING METHOD FOR BETA-SIALON | 2008 |
|
RU2384546C2 |
METHOD OF PRODUCTION OF POROUS MATERIAL | 1999 |
|
RU2191759C2 |
METHOD FOR PRODUCING HIGHLY DISPERSED SILICON CARBIDE POWDER | 2022 |
|
RU2784758C1 |
METHOD OF PRODUCING NANODISPERSED POWDER CONTAINING SILICON CARBIDE | 2023 |
|
RU2822915C1 |
METHOD OF OBTAINING MIXTURES OF HIGH-DIFFERED HETEROGENEOUS POWDERS BASED ON BORON CARBIDE | 2018 |
|
RU2683107C1 |
METHOD OF PREPARING SIALON POWDER | 2008 |
|
RU2378227C1 |
METHOD FOR OBTAINING SILICON CARBIDE | 2022 |
|
RU2789998C1 |
METHOD OF OBTAINING OF CATALYST FOR SEWAGE CLEANING FROM PHENOL, CATALYST OBTAINED BY THIS METHOD, AND METHOD OF CLEANING OF SEWAGE FROM PHENOL USING THIS CATALYST | 2013 |
|
RU2540579C2 |
Authors
Dates
2005-10-10—Published
2003-05-20—Filed