FIELD: metallurgy.
SUBSTANCE: procedure consists in degreasing chips with water solution of detergent implementing ultra-sonic bath, in washing chips in hot water, in their drying and crumbling. Also before degreasing chips are crumbled and simultaneously sprinkled with water solution of detergent; degreasing is performed in the ultra-sonic bath where concentration of detergent is 10-40 g/l at temperature 50-65°C during 5-10 minutes. Upon sizing and/or magnet separation chips can be introduced into composition of alloys as addition to charge materials.
EFFECT: increased quality of metal produced out of metal chips, and its reduced prime cost.
4 cl, 1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PROCESSING CHIPS OF REFRACTORY METALS AND ALLOYS OF TITANIUM SUBGROUP | 2003 |
|
RU2238171C1 |
PROCESSING METHOD OF METALLIC CHIPS OF TITANIUM SUBGROUP AND ITS MELTS | 2007 |
|
RU2356962C2 |
METHOD OF MAKING CASTABLE REFRACTORY NICKEL-BASED ALLOYS | 2011 |
|
RU2470081C1 |
METHOD OF PROCESSING OF HIGHLY PURE ALUMINIUM ALLOYS | 2006 |
|
RU2323984C2 |
METHOD FOR PRODUCTION OF HIGH-PURITY ZIRCONIUM OF HAFNIUM | 1993 |
|
RU2048558C1 |
CUTTING METHOD OF SEMI-FINISHED PRODUCT MADE OF ALUMINIUM ALLOY | 2007 |
|
RU2349430C2 |
METHOD FOR MANUFACTURING INGOTS OF ZIRCONIUM ALLOYS | 2022 |
|
RU2800271C1 |
PROCESS FOR PRODUCTION OF REFINED BILLETS FROM METAL OF TITANIUM GROUP AND ALLOYS ON ITS BASIS | 1996 |
|
RU2107585C1 |
METHOD OF PRODUCTION OF ZIRCONIUM-BASED ALLOYS | 2005 |
|
RU2302476C2 |
TANTALUM-BASE ALLOY REFINING METHOD | 2012 |
|
RU2499065C1 |
Authors
Dates
2010-05-20—Published
2008-10-09—Filed