FIELD: metallurgy.
SUBSTANCE: tempering method for solid alloy based on tungsten carbide involves alloy heating to the temperature over 1100°C and cooling down in tempering medium. Aqueous solution of polymer based on Termovit-M concentrate with concentration of 2-8% is used as tempering medium.
EFFECT: enhanced operational durability of tools made out of the alloy.
1 ex
Title | Year | Author | Number |
---|---|---|---|
TEMPERING METHOD OF HARD ALLOY ON BASIS OF TUNGSTEN CARBIDE | 2007 |
|
RU2355513C1 |
HARD ALLOY QUENCHING METHOD | 2005 |
|
RU2294261C1 |
TEMPERING METHOD OF HARD ALLOY | 2007 |
|
RU2356693C1 |
METHOD OF THE RAILS THERMAL TREATMENT | 2005 |
|
RU2294387C1 |
METHOD FOR HEAT TREATMENT OF CUTTING INSERTS MADE OF HARD ALLOY T5K10 | 2021 |
|
RU2759107C1 |
INDUCTION HARDENING PLANT | 2011 |
|
RU2463357C1 |
QUENCHING MEDIUM | 0 |
|
SU1756367A1 |
METHOD OF THERMAL TREATMENT OF TEETH OF DISK SAWS | 2004 |
|
RU2259408C1 |
LOW-DEFORMING QUENCHING OF ALUMINIUM ALLOYS | 2014 |
|
RU2574928C1 |
HARDENING MEDIUM | 0 |
|
SU1359313A1 |
Authors
Dates
2010-06-20—Published
2009-05-04—Filed