FIELD: metallurgy.
SUBSTANCE: modifying agent contains the following, wt %: silicone 50.0-60.0; calcium 1.5-2.5; strontium 0.2-0.3; rare-earth metals 1.5-2.5; and iron is the rest.
EFFECT: reducing the consumption of modifying agent, increasing strength of alloy processed with modifying agent.