FIELD: process engineering.
SUBSTANCE: invention relates to machine building. Method of production comprises preparing the melt, filling the melt into mould, producing casts, annealing, machining surface hardening and polishing. Surface hardening is performed by tempering at the temperature of 50…40°C lower than preset one, while one-time tempering is performed at the temperature 20…60°C lower than preset one.
EFFECT: higher efficiency of casting.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HEAT TREATMENT OF CUTTING TOOL FROM QUICK CUTTING STEELS | 2013 |
|
RU2543027C2 |
METHOD OF PRODUCING PUNCHING TOOLS AND INJECTION MOULDS FROM MOULDED BLANKS OF MARAGING STEELS | 2011 |
|
RU2448806C1 |
METHOD OF TREATMENT OF CAST HIGH-SPEED STEEL CUTTING TOOL | 0 |
|
SU850703A1 |
METHOD FOR HEAT TREATING CAST HIGH-SPEED STEEL | 0 |
|
SU1014938A1 |
METHOD OF WELDED CUTTING TOOL HEAT TREATMENT | 0 |
|
SU1770403A1 |
METHOD OF THERMAL TREATMENT OF HIGH-SPEED STEEL TOOLS | 0 |
|
SU1797626A3 |
METHOD OF HEAT TREATMENT OF HIGH-SPEED STEELS WITH INTERMETALLIDE HARDENING | 2016 |
|
RU2634548C1 |
METHOD OF TREATMENT OF HIGH-SPEED STEEL TOOLS | 0 |
|
SU737479A1 |
QUICK-CUTTING STEEL | 2001 |
|
RU2243283C2 |
QUICK-CUTTING STEEL | 2000 |
|
RU2194792C2 |
Authors
Dates
2010-12-20—Published
2009-07-10—Filed