FIELD: chemistry.
SUBSTANCE: copolyether contains an acid component (A) and at least one diol component (B). The acid component consists of 1) 50-60 mol % aromatic polyfunctional acid and 2) 40-50 mol % aliphatic acid, where 90 mol % comprises a natural long-chain dicarboxylic acid selected from azelaic acid, sebacic acid, brassilic acid or mixtures thereof. The invention enables to obtain biodegradable polyether which has over 70% biodegradability after 90 days, density equal to or less than 1.2 g/cm3, average molecular weight 40000-140000, characteristic viscosity 0.8-1.5.
EFFECT: improved characteristics of polyethers.
23 cl, 4 tbl, 9 ex
Title | Year | Author | Number |
---|---|---|---|
MULTILAYER BIODEGRADABLE FILM | 2017 |
|
RU2795428C2 |
POLYESTER COMPOSITION | 2011 |
|
RU2587167C2 |
MULTI-LAYER FILM WITH IMPROVED PROPERTIES OF ELASTIC MODULE | 2013 |
|
RU2636711C2 |
DIOL COMPOSITION AND POLYESTER | 2012 |
|
RU2591850C2 |
BIODEGRADABLE POLYESTER, METHOD FOR PRODUCTION THEREOF AND ARTICLES CONTAINING SAID POLYESTER | 2009 |
|
RU2499007C2 |
GLUE-MELT FOR GLUING THERMOSENSITIVE MATERIALS | 0 |
|
SU843764A3 |
POLYESTER POLYMERIC COMPOSITION | 2004 |
|
RU2300540C2 |
FIRE-RETARDANT POLYMER COMPOSITIONS CONTAINING DESOXYBENZOIN | 2015 |
|
RU2699361C2 |
THERMOPLASTIC POLYURETHANE HOT-MELT ADHESIVE | 2015 |
|
RU2686933C2 |
MULTILAYER FILM FOR PACKING IN VACUUM INTO TIGHT FILM, PACKING METHOD AND PACKAGES MADE BY IT | 2017 |
|
RU2737694C2 |
Authors
Dates
2011-04-10—Published
2006-03-17—Filed