FIELD: machine building.
SUBSTANCE: according to invention there is fabricated bushing out of steel. The bushing has external diametre equal to pilot diametre of the unit, while internal diametre is bigger, than nominal. After fabrication "jugged" thread is cut on internal surface of the bushing and successively this surface is rolled at a slanted net. Bronze powder is sputtered by the gas-thermal procedure onto thus prepared surface. Upon sputtering the bearing is mechanically processed.
EFFECT: reduced cost of fabrication of friction bearing at high strength of adhesion of sputtered layer with base.
1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD TO MANUFACTURE SLIDING BEARING | 2012 |
|
RU2509236C2 |
METHOD OF RECLAIMING PLAIN BEARING | 2009 |
|
RU2424888C2 |
PLAIN BEARING MANUFACTURING METHOD | 2013 |
|
RU2539515C2 |
METHOD OF SLIDING BEARING MANUFACTURING | 2018 |
|
RU2708410C1 |
METHOD OF RECONDITIONING WORN-OUT PARTS | 2012 |
|
RU2486044C1 |
METHOD OF SLIDING BEARING BUSHING MANUFACTURING | 2019 |
|
RU2734211C1 |
METHOD OF SLIDING BEARING BUSHING MANUFACTURING | 2019 |
|
RU2734210C1 |
METHOD OF PREPARING ARTICLE SURFACE FOR SPRAYING | 2009 |
|
RU2400312C1 |
SURFACE PREPARATION FOR SPUTTERING | 2012 |
|
RU2516506C2 |
METHOD OF PRODUCTION OF OILLESS BEARINGS | 2000 |
|
RU2215818C2 |
Authors
Dates
2011-04-20—Published
2009-06-24—Filed