FIELD: chemistry.
SUBSTANCE: method involves pretreatment of butadiene or butadiene nitrile rubber on plasticising equipment with further addition of vulcanising agents - sulphur, thiuram, 2-mercaptobenzothiazole, and then powdered filler, fibrous filler saturated with water-soluble epoxy resin, which is a product of the reaction of a mixture of diane and aliphatic resin with glycols or derivatives thereof. The ratio of the fibre to resin ranges from 95-5 to 60-40. A special additive of 1-5% emulsion of a liquid transition metal carbonyl in triethanolamine is then added. The material contains the following in pts.wt: rubber 100, sulphur 1-15, thiuram 0.04-0.2, 2-mercaptobenzothiazole 0.3-4.0, powdered filler 10-100, saturated fibrous filler 15-1000, metal carbonyl emulsion 0.5-10.0.
EFFECT: invention improves strength properties and wear resistance of frictional polymer materials, improves labour conditions when mixing components.
2 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING FRICTIONAL POLYMER MATERIALS | 2008 |
|
RU2419639C2 |
METHOD OF PRODUCING FRICTION POLYMER MATERIALS | 2008 |
|
RU2393177C1 |
METHOD OF ROLLING STOCK BRAKE PADS PRODUCTION | 2010 |
|
RU2463185C2 |
METHOD OF PRODUCING FRICTION POLYMER MATERIALS | 2019 |
|
RU2717055C1 |
METHOD OF PRODUCING FRICTION POLYMER MATERIALS | 2020 |
|
RU2768161C1 |
METHOD OF PREPARING FRICTION POLYMERIC MATERIALS | 1999 |
|
RU2175335C2 |
METHOD OF PREPARING FRICTIONAL POLYMER MATERIALS | 2006 |
|
RU2307841C1 |
FRICTIONAL POLYMER MATERIAL | 2008 |
|
RU2400502C2 |
METHOD FOR MAKING RUBBER GASKET-SHOCK-ABSORBER | 2001 |
|
RU2241718C2 |
METHOD OF OBTAINING ANTIFRICTION MOULDING MATERIALS | 2007 |
|
RU2330051C1 |
Authors
Dates
2011-10-10—Published
2009-08-31—Filed