FIELD: metallurgy.
SUBSTANCE: item is heated and tempered at low temperature. Also, the long-length item is continuously transferred on a transporter at rate 3-10 mm/sec. The item passes through a local zone of heating with alternative electro-magnetic field of 8-20 kHz frequency. In the local zone the item is heated to temperature 800-1000°C. Further tempering is performed to temperature 300-200°C. Local intensive cooling with a jet of compressed air facilitates formation of martensite structure of metal, where upon temperature of the item is brought to temperature of environment.
EFFECT: high efficiency and manufacture of items with different strength characteristics along section.
2 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TEMPERING THIN-WALL LONG COMPONENTS MADE OF 12X2NVFA STEEL IN CONTROLLED AIR FLOW | 2017 |
|
RU2655875C1 |
APPARATUS AND METHOD FOR HEAT TREATMENT OF A LONG-LENGTH PRODUCT WITH AN L-SHAPED PROFILE WITH A SOLE, NECK, HEAD | 2020 |
|
RU2755713C1 |
METHOD OF HIGH-QUALITY TREATMENT OF ARTICLES AND DEVICE FOR REALIZATION OF THIS METHOD | 2000 |
|
RU2201460C2 |
METHOD OF THERMAL PROCESSING OF MOULDED PARTS FROM LOW-CARBON ALLOYED STEELS | 2017 |
|
RU2639082C1 |
HARDENING METHOD OF ROLLING BEARING RINGS, AND ROLLING BEARING | 2011 |
|
RU2493269C2 |
METHOD OF HEAT TREATMENT OF STEEL RAILS | 2016 |
|
RU2644638C2 |
METHOD OF TEMPERING ALLOYED STEEL AND CAST IRON CYLINDRICAL ARTICLES | 0 |
|
SU810851A1 |
LOCAL HARDENING METHOD FOR BEARING PINS AND DEVICE FOR METHOD REALISATION | 2010 |
|
RU2439168C2 |
METHOD FOR LASER HARDENING OF WORKING SURFACES OF CUTTING TOOL EDGE | 2021 |
|
RU2781887C1 |
METHOD OF QUENCHING SPRING TERMINALS AND PLANT TO THIS END | 2011 |
|
RU2459877C1 |
Authors
Dates
2011-12-27—Published
2010-09-30—Filed