FIELD: chemistry.
SUBSTANCE: siccative is obtained by fusing 2-ethylhexanoic acid with a mixture of lead oxide (yellow lead) and cobalt hydroxide. Fusion is carried out while feeding said components simultaneously at temperature 110-120°C and molar ratio of cobalt hydroxide, lead oxide and 2-ethylhexanoic acid of 1.0:2.8-10.4:7.4-17.8, respectively. Further, a solvent white alcohol and/or nefras C4 and/or jet engine fuel TS-1 or mixture thereof is then added in amount of 50-58 wt %.
EFFECT: ensuring drying of paint materials based on alkyde, uralkyde and oily film-forming materials.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING SICCATIVE FOR PAINT MATERIALS | 2011 |
|
RU2485155C1 |
METHOD OF PRODUCING SICCATIVE FOR PAINT MATERIALS | 2011 |
|
RU2492202C1 |
METHOD OF SYNTHESIS OF SICCATIVE | 2001 |
|
RU2182916C1 |
METHOD FOR PREPARING LIGHT SICCATIVE | 2004 |
|
RU2281308C2 |
METHOD OF PREPARING MELTED LEAD-MANGANESE SICCATIVE | 1998 |
|
RU2141499C1 |
ANTICORROSION PRIMER | 2010 |
|
RU2436820C1 |
METHOD FOR PRODUCTION OF PRECIPITATED DESICCANT | 2004 |
|
RU2266939C1 |
COMPOSITION FOR COATING | 1992 |
|
RU2017779C1 |
METHOD OF OBTAINING DESICCANT | 0 |
|
SU632713A1 |
METHOD FOR PRODUCTION OF ALKYD-URETHANE ENAMEL | 2007 |
|
RU2346967C1 |
Authors
Dates
2012-05-20—Published
2010-06-22—Filed