FIELD: construction.
SUBSTANCE: in the method to prepare a binder for production of a decorative concrete including grinding, mixing, grinding of the binder, slag from melting of ferrochromium is ground to the size of 700-800 m2/kg, a hardening promoting agent - wastes of iron ores dressing with inclusions of mineral garnets in amount of 10-20% are ground to the size of 500-700 m2/kg, mixed with blast furnace pelleted slag, calcium sulfate dihydrate at the following ratio of components, wt %: blast furnace pelleted slag 28-39; calcium sulfate dihydrate 3-5; wastes of ores dressing 5-12; slag from melting of ferrochromium - balance, additionally ground to the size of 400-450 m2/kg. The binder for production of decorative concrete is characterised by the fact that it is produced by the above method.
EFFECT: higher stability of a decorative colour without reduction of strength and frost resistance of concrete on the specified binder.
2 cl, 1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
CONSTRUCTION MIXTURE FOR MAKING ROOFING SHEET AND METHOD OF MAKING ROOFING SHEET | 2011 |
|
RU2494990C2 |
BINDER | 2008 |
|
RU2368577C1 |
METHOD TO PREPARE CONCRETE | 2010 |
|
RU2462437C2 |
BINDING | 2008 |
|
RU2377200C1 |
BINDER | 2008 |
|
RU2374193C1 |
BINDER | 2008 |
|
RU2376251C1 |
BINDER | 2008 |
|
RU2363673C1 |
CLINKERLESS CEMENT | 2010 |
|
RU2430043C1 |
BINDER AND METHOD OF ITS MAKING | 2009 |
|
RU2416580C1 |
BINDING AGENT | 2000 |
|
RU2186043C2 |
Authors
Dates
2012-06-10—Published
2010-10-01—Filed