FIELD: process engineering.
SUBSTANCE: identical mechanical properties are ensured by regulation of setting finishing temperature to 1050±60°C. Note here that finishing start temperature is taken to equal 830÷890°C, rolling end temperature is taken to make 800-840°C, while temperature of sheet cooling end is taken to equal 520÷580°C.
EFFECT: improved physical properties.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING SHEETS FROM LOW-ALLOY PIPE STEEL | 2011 |
|
RU2458753C1 |
MANUFACTURING METHOD OF PLATES FROM LOW-ALLOY PIPE STEEL WITH STRENGTH CLASS K60 | 2012 |
|
RU2479639C1 |
MANUFACTURING METHOD OF PLATES FROM LOW-ALLOY PIPE STEEL WITH STRENGTH CLASS K60 | 2011 |
|
RU2465345C1 |
MANUFACTURING METHOD OF PLATES FROM LOW-ALLOY PIPE STEEL WITH STRENGTH CLASS K60 | 2012 |
|
RU2479638C1 |
METHOD MAKING SHEETS FROM LOW-ALLOY PIPE STEEL | 2011 |
|
RU2458752C1 |
MANUFACTURING METHOD OF PLATES FROM LOW-ALLOY PIPE STEEL WITH STRENGTH CLASS K60 | 2011 |
|
RU2465344C1 |
METHOD OF PRODUCING SHEETS FROM LOW-ALLOY TUBE STEEL OF K60 STRENGTH CLASS | 2011 |
|
RU2475315C1 |
METHOD OF PRODUCING LOW-ALLOY X70-GRADE PIPE STEEL | 2011 |
|
RU2458754C1 |
MANUFACTURING METHOD OF PLATES FROM LOW-ALLOY PIPE STEEL WITH STRENGTH CLASS K56 | 2011 |
|
RU2465343C1 |
METHOD OF PRODUCING SHEETS FROM LOW-ALLOYED TUBE STEEL OF X60 STRENGTH GRADE | 2011 |
|
RU2458156C1 |
Authors
Dates
2012-08-20—Published
2011-02-25—Filed