FIELD: metallurgy.
SUBSTANCE: charge includes converter sludge, scale, flux, fuel and recycling. Slag mixture together with dolomite with particle size of 0-10 mm is added as flux to the charge so that MgO content in agglomerate is within 6.9-10.5%. Fuel consumption is established based on obtaining FeO content in sinter within 7.0-13.0% at maintaining FeO/MgO ratio in it within 0.7-1.9. Charge is dosed, mixed and sintered. Utilisation of secondary raw material, obtaining of strong agglomerate of the specified composition with the properties required for normal slag formation in converter with minimum action on its lining is provided.
EFFECT: when using such agglomerate, overhaul period of converter lining is increased.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
HIGHLY BASIC AGGLOMERATE PRODUCTION METHOD AND HIGHLY BASIC AGGLOMERATE OBTAINED BY THIS METHOD | 2023 |
|
RU2808855C1 |
METHOD FOR STEEL MELTING IN CONVERTER | 2005 |
|
RU2289629C1 |
CHARGE AND METHOD OF OBTAINING FLUX AND REFRACTORY MATERIAL FOR STEEL PRODUCTION (OPTIONS) WITH ITS USE | 2020 |
|
RU2749446C1 |
STEEL SMELTING FLUX AND METHOD OF PRODUCTION OF SUCH FLUX | 2005 |
|
RU2296800C2 |
PROCESS FOR MELTING STEEL IN CONVERTER | 2001 |
|
RU2196181C1 |
AGGLOMERATE PRODUCTION METHOD | 2006 |
|
RU2337978C2 |
MIXTURE FOR PRODUCTION OF STEEL MELTING FLUX | 1998 |
|
RU2141534C1 |
MANGANESE FLUX FOR CONVERTER PRODUCTION AND CHARGE FOR PRODUCTION OF MANGANESE FLUX | 2016 |
|
RU2644838C2 |
LIME-MAGNESIAN FLUX | 1999 |
|
RU2145357C1 |
METHOD FOR SMELTING STEEL IN CONVERTER | 2005 |
|
RU2288958C1 |
Authors
Dates
2012-09-10—Published
2011-05-20—Filed