FIELD: construction.
SUBSTANCE: in the method to produce a cellular construction material, including mixing of silica-containing and alkaline components and water at the ratio of alkaline component content to content of a silica-containing component from 0.08 to 0.40 and ratio of total content of silica-containing and alkaline components to water content up to 5.3 to produce a homogeneous silicate mass, its drying and grinding, filling the mass into moulds and heating to swelling temperature in the range from 650 to 900°C with further cooldown to ambient temperature, the silicate mass after drying is ground to the particle size of 3.5-20 mm, and heating of the mass to swelling temperature is carried out at continuous temperature increase.
EFFECT: reduction of power inputs for production of a cellular construction material with preservation of its properties.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING OF POROUS CONSTRUCTION MATERIAL | 2014 |
|
RU2569138C1 |
BUILDING MATERIAL AND THE METHOD OF ITS PRODUCTION | 2006 |
|
RU2300506C1 |
METHOD FOR PRODUCTION OF CONSTRUCTION MATERIAL | 2008 |
|
RU2363685C1 |
METHOD TO PRODUCE CONSTRUCTION MATERIAL | 2012 |
|
RU2503647C1 |
WAY OF PRODUCTION OF LIGHTWEIGHT CERAMIC HEAT INSULATING AND HEAT INSULATING AND CONSTRUCTIONAL MATERIAL | 2010 |
|
RU2442762C1 |
METHOD OF MANUFACTURING LIGHT-WEIGHT CERAMIC HEAT-INSULATING AND HEAT-INSULATING-CONSTRUCTIVE MATERIAL "KONPASIT" | 2011 |
|
RU2473516C1 |
METHOD TO PRODUCE GLASS HAYDITE AND POROUS CERAMICS FROM FOSSIL MEAL AND SILICA CLAY | 2012 |
|
RU2528814C2 |
METHOD OF PRODUCING HEAT-INSULATING MATERIAL - FOAM GLASS AND MIXTURE FOR PRODUCTION THEREOF | 2017 |
|
RU2671582C1 |
METHOD FOR OBTAINING CONSTRUCTION MATERIAL | 2007 |
|
RU2333176C1 |
CONSTRUCTION MATERIAL AND METHOD OF ITS PRODUCTION | 2007 |
|
RU2348596C1 |
Authors
Dates
2012-10-20—Published
2010-10-19—Filed