FIELD: metallurgy.
SUBSTANCE: method involves out-of-surface metal working at "furnace-ladle" unit. After molten metal is supplied to the above unit, covering slag is removed from steel-pouring ladle; new slag is induced by addition of lime and fluor spar in the ratio of (4…5):1 with total material consumption of 7…12 kg/t. Then, steel deoxidation is performed with primary aluminium on the basis of obtaining the content of acid-soluble aluminium of not less than 0.080%, metal heating to temperature of not less than 1620°C. After that, fluidised lime is injected in quantity of 2.8…4.2 kg/t.
EFFECT: use of invention provides the required desulphuration degree of steel without growth of silicon content during processing.
Title | Year | Author | Number |
---|---|---|---|
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
METHOD OF DRY STEEL PRODUCTION | 2013 |
|
RU2533263C1 |
METHOD OF OUT-OF-FURNACE TREATMENT OF STEEL IN LADLE | 2020 |
|
RU2735697C1 |
OUT-OF-FURNACE STEEL TREATMENT METHOD | 2010 |
|
RU2440421C1 |
OUT-OF-FURNACE STEEL TREATMENT METHOD | 2010 |
|
RU2440422C1 |
METHOD OF PRODUCING LOW-SILICON STEEL | 1999 |
|
RU2166550C2 |
STEEL-MAKING METHOD IN ARC ELECTRIC STEEL-SMELTING FURNACE | 2008 |
|
RU2384627C1 |
METHOD OF PRODUCING STEEL WITH SPECIFIED LIMIT ON SULPHUR CONTENT | 2023 |
|
RU2816888C1 |
METHOD FOR OFF-FURNACE STEEL TREATMENT | 2015 |
|
RU2607877C2 |
METHOD OF ALLOYING STAINLESS STEEL WITH TITANIUM | 2002 |
|
RU2226555C2 |
Authors
Dates
2012-10-27—Published
2011-07-08—Filed