FIELD: process engineering.
SUBSTANCE: invention relates to woodworking. Propose method comprises wood blank preliminary shaping and sizing and adjusting moisture content. Blank is impregnated with polymerisation composition and subjected to drying and cooling. Note here that said blank is subjected to drying in vacuum pressure chamber to moisture content of 2-3% and to vacuum of 0.8 MPa for 45-60 min. Blank is immersed in impregnation solution, for example, 20-25%-solution of acetone-formaldehyde resin taken in amount sufficient for deep immersion. Vacuum of 0.8 MPa is created to keep wood blank in said solution for 30-60 min. Hydraulic pressure of 8-10 MPa is created in vacuum pressure chamber for 2-3 h. Unused impregnation solution of wood modifier is pumped over into standby tank. Vacuum of 0.8 MPa is created in vacuum pressure chamber and retained for 0.5-1.0 h. Pressure is said chamber is recovered to barometric pressure to dry impregnated wood blank to moisture content of 5-8%.
EFFECT: improved hardwood properties.
6 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERISATION-IMPREGNATION SOLUTION FOR WOOD MODIFICATION | 2011 |
|
RU2479422C2 |
COMPOSITION FOR WOOD MODIFYING | 1992 |
|
RU2065355C1 |
METHOD OF TIMBER IMPREGNATION | 2017 |
|
RU2646612C1 |
METHOD FOR PRODUCTION OF MODIFIED WOOD | 2007 |
|
RU2346809C2 |
IMPREGNATING FIREPROOF COMPOSITION | 1999 |
|
RU2147028C1 |
METHOD FOR MANUFACTURING WOOD NEUTRON SHIELDING MATERIAL | 2022 |
|
RU2792345C1 |
COMPOSITION FOR PREPARING SOLUTION FOR WOOD IMPREGNATION, SOLUTION FOR WOOD IMPREGNATION AND METHOD FOR USING THIS SOLUTION | 2021 |
|
RU2771676C1 |
METHOD FOR MAKING PRESSED MODIFIED WOOD | 1992 |
|
RU2024667C1 |
LUMBER WORKING AND DEVICE TO THIS END | 2011 |
|
RU2516259C2 |
METHOD OF DEEP IMPREGNATION OF WOOD | 2011 |
|
RU2469842C1 |
Authors
Dates
2013-02-10—Published
2011-07-27—Filed