FIELD: metallurgy.
SUBSTANCE: method involves charge melting from cobalt oxides and carbon reducing agent, reduction and decarburisation of cobalt after complete melting. Melting is performed at content of carbon reducing agent in the charge of 16-21 wt %. Decarburisation is performed at the arc current force of 90-95% of its maximum value. When carbon concentration in cobalt reaches 0.3%, current force is set to maximum and equals to 6.3 kA.
EFFECT: increasing specific performance of the process and reducing specific power consumption.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR DEPLETION OF NICKEL-COBALT CONVERTER SLAGS | 2004 |
|
RU2258754C1 |
METHOD OF PREPARING NICKEL-CONTAINING ADDITION ALLOY | 1996 |
|
RU2095427C1 |
METHOD OF STEEL PRODUCTION IN ELECTRIC ARC FURNACE | 2015 |
|
RU2610975C2 |
METHOD FOR LIQUID-PHASE OBTAINING OF DIRECT-REDUCED IRON | 2012 |
|
RU2511419C2 |
METHOD OF PRODUCING STANDARD ELECTROCORUNDUM | 0 |
|
SU1710507A1 |
METHOD OF CARBO-THERMAL REDUCTION OF SILICON | 2008 |
|
RU2383493C1 |
METHOD FOR PRODUCING VANADIUM-MANGANESE-SILICON MASTER ALLOY | 2016 |
|
RU2633678C1 |
METHOD OF PRODUCTION OF FERROVANADIUM | 1997 |
|
RU2112070C1 |
MELTING METHOD OF FERROSILICON IN ORE HEAT-TREATMENT FURNACE | 2010 |
|
RU2451098C2 |
METHOD OF RECEIVING OF VANADIUM-BEARING ALLOYS AND LIGATURES | 2007 |
|
RU2368689C2 |
Authors
Dates
2013-02-27—Published
2011-05-20—Filed