FIELD: metallurgy.
SUBSTANCE: in compliance with this method, flushing is performed by the mix of nitrogen with oxygen at flow rate of 0.7-1.2 l per one kg of remelted consumable electrode at 1.43-2.45 l/min while amount of oxygen in said mix is kept equal to 0.5-10 vol. % of total amount of mix blown into slag bed.
EFFECT: power savings, higher quality of cast ingot.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF INGOTS FROM CHIPS | 1991 |
|
RU2013457C1 |
METHOD OF STEEL DEOXIDATION IN ELECTROSLAG REMELTING | 2013 |
|
RU2541333C1 |
PROCEDURE FOR ELECTRIC-SLAG REMELTING | 2009 |
|
RU2424335C1 |
ELECTROSLAG REMELTING METHOD AND DEVICE FOR ITS IMPLEMENTATION | 2009 |
|
RU2448173C2 |
METHOD FOR STEEL DEOXIDATION DURING ELECTROSLAG REMELTING | 2016 |
|
RU2630100C1 |
PROCEDURE FOR HOLLOW INGOT ELECTRIC SLAG MELTING | 2009 |
|
RU2424325C2 |
ELECTRIC SLAGGY FURNACE FOR REMELTING | 2007 |
|
RU2348710C2 |
FLUX FOR ELECTROSLAG SMELTING OF SOLID AND HOLLOW INGOTS FROM BORON-CONTAINING STEELS | 2017 |
|
RU2656910C1 |
METHOD FOR ELECTROSLAG REMELTING | 2011 |
|
RU2487182C1 |
METHOD OF ELECTROSLAG MELTING OF FERROTITANIUM | 2007 |
|
RU2346994C2 |
Authors
Dates
2013-05-27—Published
2012-04-06—Filed