FIELD: chemistry.
SUBSTANCE: invention relates to a method of making fuel briquettes, which involves mixing carbon filler with ground coal, adding a binding substance and briquetting the mixture under pressure. The carbon filler, which is in form of aluminium wastes, anode paste and electrodes in amount of 25.1-85.00 wt %, is dry-mixed with ground brown coal until a 100% dry mass is obtained, followed by addition of the binding substance to the dry mass. The binding substance used is bitumen or polyvinyl alcohol in amount of 2-10 wt %, in excess of 100% of the dry mass. If polyvinyl alcohol is used as the binder, hydrophobic additives are added to the obtained mixture in amount of 1-5 wt %, in excess of 100% of the obtained mixture.
EFFECT: improved properties.
3 cl, 3 tbl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING LUMP FUEL | 2018 |
|
RU2666738C1 |
METHOD OF PRODUCING FUEL BRIQUETTES | 2015 |
|
RU2601743C1 |
METHOD OF PRODUCING FUEL BRIQUETTES | 2018 |
|
RU2693043C1 |
PROCESS FOR PRODUCING FUEL BRIQUETTES | 1992 |
|
RU2005770C1 |
METHOD FOR PRODUCING SMOKELESS HOUSEHOLD FUEL | 2020 |
|
RU2747049C1 |
METHOD OF OBTAINING SMOKELESS HOUSEHOLD FUEL | 2018 |
|
RU2673794C1 |
FUEL BRIQUETTE | 2019 |
|
RU2733946C1 |
METHOD OF PRODUCING FUEL BRIQUETTE | 2019 |
|
RU2733947C1 |
METHOD OF PRODUCING MINERAL WOOL | 2019 |
|
RU2730462C1 |
COMPOSITION OF CHEMICALLY OBTAINED BINDING AGENT FOR MANUFACTURE OF COAL BRIQUETTES | 2011 |
|
RU2472845C2 |
Authors
Dates
2013-06-27—Published
2012-03-01—Filed