FIELD: metallurgy.
SUBSTANCE: proposed composition contains the following substances, in wt %: carbon 0.27 - 0.32, titanium 5.8 - 6.2, nickel 0.5 - 0.9, titanium carbide (TiC) 0.5 -1.5, iron making the rest. Besides, it may contain up to 0.05% traces of manganese, 0.15 - 0.17% of silicon, and ≈0.03% of sulfur and phosphorus. Titanium carbide is added in the form of powder with particle size of up to 10 mcm into ladle or in melt jet in teeming steel into metallic chill mould.
EFFECT: improved processing and operating properties, lower costs.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING CAST DISPERSION-HARDENING FERRITE-CARBIDE STEEL | 2015 |
|
RU2605017C1 |
METHOD OF OBTAINING CAST BIMETALLIC STAMPS OF THE SYSTEM “FERRITIC CARBIDE STEEL - AUSTENITE-BAINITE CAST IRON” | 2018 |
|
RU2677645C1 |
METHOD OF PRODUCTION OF CAST BIMETALLIC MOULDS OF FERRITE STEEL-ALUMINIUM CAST IRON ALLOY | 2012 |
|
RU2507026C2 |
DIE STEEL | 0 |
|
SU1724723A1 |
STEEL | 1999 |
|
RU2144094C1 |
DIE ALLOY | 2011 |
|
RU2479664C1 |
DIE ALLOY | 2020 |
|
RU2727463C1 |
CAST PRESSED STEEL | 1996 |
|
RU2095460C1 |
INSTRUMENT STEEL FOR HOT DEFORMATION | 2013 |
|
RU2535148C2 |
BEARING CAST IRON | 2008 |
|
RU2365659C1 |
Authors
Dates
2013-07-20—Published
2011-03-11—Filed