FIELD: metallurgy.
SUBSTANCE: "ЖС32" or "ЖС32МОНО" alloy is used for bonding of at least two part fragments from said alloy by diffusion conglomeration with application of 11 g/mm2 load in vacuum at 1320°C for 40 min to 1 hour.
EFFECT: high mechanical strength and accurate sizes.
7 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
DIFFUSION WELDING OF NICKEL-BASED CASTABLE REFRACTORY ALLOY | 2014 |
|
RU2558692C1 |
METHOD OF DIFFUSION WELDING OF "BLISK"-TYPE GAB TURBINE ROTOR MADE FROM HEAT-PROOF NICKEL ALLOYS | 2009 |
|
RU2414350C1 |
BLADE SURFACE PROTECTION METHOD | 2003 |
|
RU2252110C1 |
METHOD OF PROTECTION OF THE BLADES OF THE GASEOUS TURBINES | 2004 |
|
RU2280096C1 |
TURBOMACHINES BLADES SHROUDS FROM HEAT-RESISTANT NICKEL ALLOYS RECONSTRUCTION METHOD | 2017 |
|
RU2667110C1 |
TREATMENT METHOD OF MOULDINGS WITH SINGLE-CRYSTAL FROM HEAT-RESISTANT NICKEL ALLOYS BY HOT ISOSTATIC PRESSING | 2008 |
|
RU2380454C1 |
METHOD FOR MAKING ROTOR OF GAS TURBINE ENGINE | 2001 |
|
RU2196672C1 |
METHOD OF TREATMENT OF AN ARTICLE WITH AN EQUIAXIAL STRUCTURE MADE OUT OF A HEAT-RESISTANT ALLOY | 2003 |
|
RU2261935C2 |
METHOD FOR FORMING MEMBER OF TURBINE IMPELLER AND TURBINE IMPELLER | 2004 |
|
RU2265497C1 |
MATERIAL OF CERAMIC LAYER OF HEAT PROTECTING COATING | 2013 |
|
RU2556248C1 |
Authors
Dates
2013-09-27—Published
2011-10-07—Filed