FIELD: chemistry.
SUBSTANCE: composite material consists of the following, wt %: polyethylene 277 50-55 and a copper polyacrylamide polycomplex 50-45. The copper polyacrylamide polycomplex is obtained by dissolving copper powder in ammonia solution, mixing the obtained solution with aqueous polyacrylamide solution and separating the polycomplex from the solution with acetone or ethyl alcohol.
EFFECT: longer service life of friction assemblies operating in a dry environment, high hardness of articles.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
ANTIFRICTION COMPOSITE MATERIAL | 2012 |
|
RU2495060C1 |
POLYAMIDE COMPOSITION AND METHOD FOR PREPARATION THEREOF | 2011 |
|
RU2488613C2 |
ANTIFRICTION POLYMER COMPOSITION | 2010 |
|
RU2445323C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF COMPOSITE NICKEL COATINGS | 2013 |
|
RU2524462C1 |
ANTIFRICTIONAL POLYMER COMPOSITION WITH THERMALLY EXPANDED GRAPHITE | 2013 |
|
RU2535216C1 |
METHOD OF PRODUCING POLYMERIC NANOCOMPOSITE MATERIAL AND MATERIAL PRODUCED USING SAID METHOD | 2008 |
|
RU2403269C2 |
FLUOROPLASTIC-BASED ANTIFRICTION POLYMER COMPOSITION | 2017 |
|
RU2665429C1 |
PRODUCTION OF COMPOSITE COATINGS ON GATE METAL ALLOYS | 2013 |
|
RU2527110C1 |
ANTIFRICTIONAL COMPOSITE POWDERED MATERIAL | 2006 |
|
RU2331685C2 |
ANTIFRICTION MATERIAL "ROMANIT", METHOD OF PREPARATION THEREOF, AND FRICTION UNIT MEMBER | 2001 |
|
RU2201431C2 |
Authors
Dates
2014-01-20—Published
2012-06-20—Filed