FIELD: metallurgy.
SUBSTANCE: tungsten-containing raw material and solution of sodium carbonate with concentration of 220 g/l is loaded to an autoclave. A leaching process is performed during at least 6 hours at the temperature of 200-225°C with constant mixing.
EFFECT: possible processing of raw material with tungsten content.
2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING AMMONIUM PARATUNGSTATE | 2015 |
|
RU2600045C1 |
METHOD FOR OBTAINING AMMONIUM TUNGSTATE | 2012 |
|
RU2506331C1 |
WOLFRAMITE CONCENTRATE PROCESSING METHOD | 2005 |
|
RU2293132C1 |
METHOD OF PROCESSING TUNGSTEN CONCENTRATES | 2015 |
|
RU2605741C1 |
AMMONIUM PARATUNGSTATE PRODUCTION PROCESS | 1996 |
|
RU2118668C1 |
METHOD FOR PROCESSING SOLUTIONS AFTER CARBONATE PROCESSING OF TUNGSTEN ORES | 2016 |
|
RU2633677C1 |
METHOD OF HYDROMETALLURGICAL PROCESSING OF TUNGSTEN CONCENTRATES | 1998 |
|
RU2149200C1 |
METHOD FOR EXTRACTION OF MOLYBDENUM FROM TUNGSTEN-CONTAINING SOLUTIONS | 1992 |
|
RU2048560C1 |
METHOD FOR PROCESSING OF WOLFRAMITE | 1995 |
|
RU2094511C1 |
PROCESSING OF GOLD-BEARING CONCENTRATES OF TWO-FOLD HARDNESS | 2012 |
|
RU2514900C2 |
Authors
Dates
2014-01-20—Published
2012-11-19—Filed