FIELD: chemistry.
SUBSTANCE: method of producing green heat-absorbing glass is carried out by controlling the redox potential of glass mass by adding a mixture of oxidising agents and reducing agents to the charge mixture: oxidising agents - sodium sulphate and sodium nitrate (Na2SO4+NaNO3) in total amount of 10.0-12.5 kg per ton of glass mass, with the ratio (Na2SO4:NaNO3)=(4-2):1 and a carbon (C) reducing agent with the ratio (Na2SO4+NaNO3):C=1:(0.02-0.025). Additional dyes from the family Cr2O3, CuO, Pr2O3, V2O5 can also be added to the charge mixture, with the following content thereof in the glass, wt%: Cr2O3 - 0-0.03; CuO - 0-0.25; Pr2O3 - 0-0.07; V2O5 - 0-0.08 and mixtures thereof. Said glass has a visible light transmission coefficient (TV)≥70% and full solar energy transmission coefficient (TS)≤50% with dominant wavelength λd of 498-530 nm and degree of reduction of Fe2O3 therein to FeO of 25-30%.
EFFECT: obtaining green heat-absorbing glass for vehicles and construction.
3 cl, 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
BLUE GLASS AND A METHOD FOR PRODUCTION THEREOF | 2018 |
|
RU2696742C1 |
METHOD OF MANUFACTURING GREENISH-BLUE, AMBER, BRONZE, GRAY, LILAC AND ROSE- COLORED HEAT-ABSORBING GLASS | 1998 |
|
RU2136619C1 |
METHOD OF MANUFACTURING GREEN HEAT-ABSORBING GLASS | 2000 |
|
RU2178393C2 |
METHOD OF PRODUCTION OF GLASS COLOURED IN MASS | 2006 |
|
RU2330820C1 |
METHOD FOR MAKING HEAT ABSORBING GLASS | 0 |
|
SU1135716A1 |
SODA-CALCIUM-SILICATE GLASS WITH HIGH VISIBLE LIGHT TRANSMITTANCE | 2020 |
|
RU2816148C1 |
METHOD OF PRODUCTION OF GLASS | 2005 |
|
RU2301783C2 |
GREEN GLASS | 1990 |
|
RU2067559C1 |
GLASS WITH HIGH PERMEABILITY | 2011 |
|
RU2634872C1 |
CHARGE AND GLASS COMPOSITION FOR GLASS-CRYSTAL MATERIAL | 2021 |
|
RU2781058C1 |
Authors
Dates
2014-05-10—Published
2012-12-06—Filed