GLASS WITH HIGH PERMEABILITY Russian patent published in 2017 - IPC C03C3/87 C03C4/10 

Abstract RU 2634872 C1

FIELD: chemistry.

SUBSTANCE: glass contains the following components, wt %: SiO2 65-75; Na2O 10- 20; CaO 5-15; MgO 0-5; Al2O3 0- 5; K2O 0-5; MnO2 0.15-0.6; FeO 0.0010-0.0030; Fe2O3 (total iron) 0.001-0.03. Glass has an oxidation-reduction ratio in the range of 0.1 to 0.4.

EFFECT: increased permeability of energy of visible and infrared light.

8 cl, 4 dwg, 4 tbl

Similar patents RU2634872C1

Title Year Author Number
LITHIUM-CONTAINING GLASS WITH HIGH CONTENT OF OXIDATIVE IRON AND METHOD FOR PRODUCTION THEREOF 2013
  • Gudvin Dzhordzh B.
  • Arbab Mekhran
  • Kherris Kerolajn S.
  • Shelestak Larri Dzh.
RU2580857C1
SODA-CALCIUM-SILICATE GLASS WITH HIGH VISIBLE LIGHT TRANSMITTANCE 2020
  • Cid-Aguilar, Jose, Guadalupe
  • Haskins, David, R.
  • Buchanan, Michael, J.
RU2816148C1
METHOD OF PRODUCING GREEN HEAT-ABSORBING GLASS FOR VEHICLES AND CONSTRUCTION 2012
  • Zhimalov Aleksandr Borisovich
  • Gorina Inessa Nikolaevna
  • Polkan Galina Alekseevna
  • Bondareva Lidija Nikolaevna
RU2514868C1
BLUE GLASS AND A METHOD FOR PRODUCTION THEREOF 2018
  • Ablyazov Kamil Alimovich
  • Zhimalov Aleksandr Borisovich
  • Gorina Inessa Nikolaevna
  • Bondareva Lidiya Nikolaevna
  • Polkan Galina Alekseevna
  • Zavarina Svetlana Viktorovna
  • Gerancheva Olga Evgenevna
RU2696742C1
SOLAR CELL USING ULTRA-TRANSPARENT LOW-IRON GLASS 2007
  • Tomsen Skott V.
  • Khul'M Richard
  • Lenda Leonid M.
RU2412121C2
BLUE GLASS WEAKLY ABSORBING SOLAR RADIATION 2007
  • Khejtoff Robert B.
  • Majner Glen T.
RU2429209C2
DARK TINTED WINDOW 2012
  • Shelestak Lehrri Dzh.
  • Til' Dzhejms P.
RU2551152C2
METHOD OF REDUCING REDOX-RATIO OF GALSS MASS AND OBTAINED THEREOF SUPERTRANSPARENT GLASS 2009
  • Shelestak Lehrri Dzh.
  • Shvenninger Ronal'D L.
RU2536526C2
GRAY GLASS COMPOSITION 2007
  • Khul'M Richard
  • Tomsen Skott V.
RU2458869C2
COMPOSITION OF GREY GLASS 2006
  • Shelestak Lehrri Dzh.
  • Smit Dennis Dzh.
  • Boldof Dzhejms M.
RU2430024C2

RU 2 634 872 C1

Authors

Shelestak Lerri Dzh.

Dates

2017-11-07Published

2011-09-01Filed