FIELD: chemistry.
SUBSTANCE: electrodeposited layer of an iron-chromium coating undergoes carbonitriding for 1-4 hours at 600-650°C using a paste of the following composition, wt %: potassium ferrocyanide 40, sodium carbonate 10, calcium carbonate 5, soot 45.
EFFECT: high microhardness and wear resistance of steel components.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HARDENING OF METALLIC SURFACES | 2004 |
|
RU2261939C1 |
METHOD OF HARDENING ELECTRODEPOSITED IRON-CHROMIUM COATINGS BY CARBONISATION | 2013 |
|
RU2537471C2 |
METHOD OF CARBONITRIDING PARTS MADE FROM STRUCTURAL AND TOOL STEELS | 2015 |
|
RU2600612C1 |
CARBONITRIDING OF PARTS FROM DIE STEELS | 2011 |
|
RU2501884C2 |
CYANIDATION METHOD OF STEEL OR TITANIC PRODUCTS | 2007 |
|
RU2349432C2 |
METHOD OF CARBONITRIDING PARTS MADE FROM STRUCTURAL AND TOOL STEELS | 2015 |
|
RU2592339C1 |
METHOD OF CARBONITRIDING METALS IN PASTES | 2003 |
|
RU2254396C1 |
STRENGTHENING METHOD OF METALLIC SURFACES SULPHOCYANIDING | 2007 |
|
RU2355815C2 |
METHOD OF CARBONITRIDING PARTS MADE FROM STRUCTURAL AND TOOL STEELS | 2015 |
|
RU2586178C1 |
CARBONITRIDING OF PARTS FROM DIE STEELS | 2014 |
|
RU2574943C1 |
Authors
Dates
2014-07-27—Published
2013-03-07—Filed