FIELD: metallurgy.
SUBSTANCE: invention relates to field of strengthening of restored surfaces of steel details. Method includes sulphocyaniding of electrodeposited coating iron - boron during 1 - 3 h at temperature 550 - 600 °C with usage of plaster of the following composition, wt %: iron pyrites 25, potassium ferrocyanide 55, chamotte 20.
EFFECT: increasing of microhardness and wear resistance of steel details.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HARD FACING OF STEEL PARTS BY SULPHIDISING | 2007 |
|
RU2360038C2 |
METHOD OF HARDENING OF METALLIC SURFACES | 2004 |
|
RU2261939C1 |
METHOD OF HARDENING ELECTRODEPOSITED IRON-CHROMIUM COATINGS BY CARBONITRIDING | 2013 |
|
RU2524294C1 |
METHOD OF HARDENING ELECTRODEPOSITED IRON-CHROMIUM COATINGS BY CARBONISATION | 2013 |
|
RU2537471C2 |
METHOD OF ELECTROLYTIC DEPOSTION OF IRON-VANADIUM-COBALT ALLOY | 2009 |
|
RU2401328C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
ELECTROLYTE FOR COAT DEPOSITION | 2003 |
|
RU2250935C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
METHOD OF ELECTROLYTIC PRECIPITATION OF IRON-MOLYBDENUM DISULFIDE COATING | 2013 |
|
RU2537686C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
Authors
Dates
2009-05-20—Published
2007-04-09—Filed