FIELD: chemistry.
SUBSTANCE: binder contains bitumen, a product of alcoholysis of elastic polyurethane foam wastes and an isocyanate component. Components are in the following ratio, pts.wt: bitumen 100, product of alcoholysis of elastic polyurethane foam wastes 5-13, isocyanate component 4-12. The binder is obtained by heating petroleum bitumen to temperature of 90-110°C, adding the required amount of the product of alcoholysis of elastic polyurethane foam wastes while mixing constantly; mixing is carried out for 10-60 minutes; the required amount of the isocyanate component is added, after which the binder is mixed for another 10-30 minutes at the same temperature. The method of preparing the binder is highly efficient and safe.
EFFECT: high softening temperature, hardness, elasticity and flexibility at low temperatures.
2 cl, 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF GETTING A POLYMER-BITUMEN BENDING BASED ON FOAMED POLYURETHANE | 2017 |
|
RU2648097C1 |
BITUMEN MODIFICATION PROCESS | 2005 |
|
RU2296142C2 |
COMPOSITE RUBBER-BITUMINOUS BINDER AND METHOD OF ITS OBTAINING | 2016 |
|
RU2655334C2 |
METHOD TO PREPARE RUBBER MODIFIED BITUMEN | 2012 |
|
RU2489464C1 |
MODIFIER OF ORGANIC BINDER | 2014 |
|
RU2583016C2 |
ASPHALT-POLYMER BINDER | 2000 |
|
RU2181733C2 |
METHOD OF PREPARING BITUMEN-BUTYL RUBBER CONCRETE | 2000 |
|
RU2174133C1 |
METHOD OF PRODUCTION OF THE POLYMERIC-BITUMINOUS COMPOSITION | 2004 |
|
RU2276116C1 |
WATERPROOF POLYMER-BITUMEN EMULSION COMPOUND | 2013 |
|
RU2521634C1 |
BITUMEN COMPOSITION | 2004 |
|
RU2267506C1 |
Authors
Dates
2014-08-27—Published
2013-03-22—Filed