FIELD: chemistry.
SUBSTANCE: glass includes components with the following ratio, wt %: PbO 75.9-78.5; PbF2 3.9-6.3; B2O3 7.7-7.8; SiO2 0.75-1.5; ZnO 4.3-5.1; Cu2O 0.75-1.5; Bi2O3 1.0-2.0; CdO 1.0-2.0. Coefficient of linear thermal expansion of glass is 105·10-7K-1. Temperature of welding is 480-490°C.
EFFECT: increased temperature of welding and sealing for increase of upper limit of working temperature of piezoresonance devices.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
LOW-MELTING GLASS | 1998 |
|
RU2152909C2 |
GLASS FOR GLASS CERAMIC CEMENT | 2003 |
|
RU2237624C1 |
LOW-MELTING GLASS | 2003 |
|
RU2237623C1 |
FUSIBLE GLASS | 2000 |
|
RU2185343C2 |
EASILY FUSIBLE GLASS COMPOSITION PRODUCTION METHOD | 2016 |
|
RU2614844C1 |
COMPOSITION OF EASILY FUSIBLE GLASS CERAMIC MATERIAL | 2000 |
|
RU2197441C2 |
LOW-MELTING GLASS FOR MAGNETIC HEADS | 1988 |
|
SU1533244A1 |
COMPOSITION FOR LOW-MELTING SOLDERING MATERIAL | 1991 |
|
RU2053211C1 |
GLASS FOR GLASS CERAMIC CEMENT | 2000 |
|
RU2188171C2 |
FUSIBLE GLASS FOR CONNECTION OF PARTS | 1990 |
|
SU1736107A1 |
Authors
Dates
2015-02-10—Published
2013-07-01—Filed